Apply a coat of varnish on the floor to smoothen the surface.
Epoxy pebble stone flooring kit.
Our epoxy is made for pebblestone river rock stone 1 bag of pebbelstone river rock is 50lbs 1 gallon kit of epoxy will cover 30 sq ft 1 50lb bag of pebblestone covers 10 12 sq ft we do not stock pebblestone at the office only at plant will have to be shipped.
This kit does not contain pumps.
This kit contains 1 gallon resin and gallon hardener.
Is a system where small pebbles are mixed with epoxy resin to create a beautiful and durable nonskid coating.
Is a system where small pebbles are mixed with epoxy resin to create a beautiful and durable nonskid coating.
Let it dry completely.
Step 4 mix the pebbles with epoxy resin.
Aeromarine products rock and pebble paving epoxy 1 1 2 gallon kit.
The mixed kit produces a total of 1 1 2 gallons of epoxy resin that has a work life of 30 minutes and a cure time of 24 hours at 70 degrees f.
Separately mix the pebbles with the epoxy resin and spread the mixture across the floor until you have covered the floor completely.
Pebble paving flooring patio decks driveway etc.
The next step is to scrape off any stray pebbles that ahre sticking up and sweep or blow off the floor to remove the extra pebbles.
Then mix up some more polyavastic or epoxy and roll a topcoat over the floor.
It has become even more popular recently because the frozen yogurt chain called pinkberry s uses the system for their restaurant floors.
Let it dry for 24 hours.
Price range 0 00 100 00 1 100 00 200 00 2 200 00 400 00 2.
Allow your diy epoxy stone flooring to fully cure.